No.
|
Problem
|
Solution / Remedy
|
|
01
|
Under deposit corrosion
|
ALTRET CMC increases Ash fusion temperature and reduce fouling tendency and thereby control Under deposit corrosion
|
|
02
|
Fouling tendency
|
ALTRET CMC product minimizes fouling tendency as it changes Ash particle morphology also reduce angle of repose.
|
|
03.
|
Conductivity of Ash
|
ALTRET CMC influences ash conductivity and thus minimizes SPM.
|
|
04
|
Ash Density
|
Reduce as ALTRET product will change ash particle morphology
|
|
05
|
CO, NOx, Sox
|
Reduces due to the anti emission
Characteristic of ALTRET CMC
|
|
06
|
Unburnt
|
Decrease due to the combustion catalyst effect of ALTRET CMC.
|
|
07
|
Erosion rate
|
Minimizes Due to changes in ash morphology
|
|